• Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
  • Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
  • Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
  • Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
  • Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
  • Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

Refractoriness (℃): 1770< Refractoriness< 2000
Feature: Long Time Materials
Shape: Granule/Powder
Material: Silicon Carbide (SiC)
Application: Abrasive Tools, Refractory, Ceramics,etc
Color: Green
Samples:
US$ 20/kg 1 kg(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2019

Suppliers with verified business licenses

Group Corporation
  • Overview
  • Product Description
  • Product Parameters
  • Detailed Photos
  • Production Process
  • Packaging & Shipping
  • Application
  • After Sales Service
Overview

Basic Info.

Model NO.
silicon carbide
Other Name
Carborundum, Emery
Abrasive Grain Sizes
0-1,1-3,3-5,0-10mm, F12-F220, Customized
Transport Package
25kg/Bag, Jumbo Bag or Customized
Specification
custom-made
Trademark
XS
Origin
Hebei, China
HS Code
2849200000
Production Capacity
2000 Metric Ton/Month

Product Description

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

 

Product Description

Silicon carbide is an inorganic substance with a chemical formula of SiC. It is made by high temperature smelting of raw materials such as quartz sand, petroleum coke (or coal coke), and wood chips (salt is needed to produce green silicon carbide) through a resistance furnace. Silicon carbide also exists in nature, a rare mineral, moissanite. Among the non-oxide high-tech refractory materials such as C, N, and B, silicon carbide is the most widely used and most economical one.
 

Product Parameters

 
Grit Size
Chemical Composition%(by weight)
SIC
F.C
Fe2O3
12#~90#
≥99.00
≤0.20
≤0.20
100#~180#
≥98.50
≤0.25
≤0.50
220#~240#
≥97.50
≤0.25
≤0.70
W63~W20
≥97.00
≤0.30
≤0.70
W14~W10
≥95.00
≤0.30
≤0.70
W7~W5
≥94.00
≤0.50
≤0.70
Item Black silicon carbide Green silicon carbide
Basic mineral α-SIC α-SIC
Crystal system hexagonal hexahonal
Crystal color Black Green
Density ≥3.12g/cm3 ≥3.18g/cm3
Mohs hardness 9.15 9.15
Micro hardness HV3100-3280 HV3200-3400
Grinding ability(compared with diamond as one) 0.25 0.28
Liner expansion coefficient when 900ºC.α·10-6k-1 4.4 4.6
Electrical resistivity 3×105-3×107Ω.cm 3×105-3×107Ω.cm

Size: 0-1mm; 0-3mm; 0-10mm; 1-10mm; etc

Detailed Photos

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

 

Production Process

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

Packaging & Shipping

 

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

Application

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing

Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
Good Thermal Conductivity Green Silicon Carbide Powder for Semiconductor Piezoelectric Crystal Grinding and Polishing
                                                   UV detectors                                                                    Light emitting diodes (LEDs)

After Sales Service

1. 7*24 hours on-line service.
2. Continuously monitor customers' usage.
3. Engineers on site for after-sale retun visit and providing techinical support.
4. Strong production capacity and plenty of inventory to ensure further orders.


 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Diamond Member Since 2019

Suppliers with verified business licenses

Group Corporation
Registered Capital
5000000 RMB
Plant Area
101~500 square meters